Trouble
Cause
Solution
Pigment dissolves or breaks down in the fountain solution causing a light discoloration of the non-printing areas.

 




INK

Too low in viscosity to carry the pigment, varnish is not water resistant.

Pigment is hydrophilic and bleeds in water and alcohol.



 

Add a high viscosity varnish to the ink.

Reformulate ink with water and alcohol resistant pigments.

 

PAPER

Contain solustion is extracting an emulsifier or sensitizing agent from the paper coating.
Proof : substitution of another paper stops the tinting.

 

Replacement of paper.

  PRESS

Too much acid in fountain solution

 

Check PH of fountain solution and reduce acidity. Reduce amount of solution

 

 

Copyright 2001 A.S INK All rights reserved.